I removed our bike rack factory installed 1.5" receiver and noticed some corrosion on the underside of the rack where the u-bolts/washer attach .  Will be checking other fasteners / washers going through the aluminum members around the bumper/bike rack area and adding some thin delrin/acetal washers to put under the stainless washers and maybe adding a thin coat of Ultra Tef-Gel to the hole walls  -OR- should I do something different? 

image.png.efe49abb81ba75e2fcd10e44d69ce4e0.png

SE Texas  | 2021 Elite II  Twin Bed # 927  "Lucy"  |  2019 F250 FX4 6.7

Oliver Travel Trailer for Sale
Find Oliver Travel Trailers for Sale
New Travel Trailers for Sale
Posted

Corrosion between dis-similar metal is common in the boating world.  Very common to find severe corrosion between, say, a 6061 aluminum mast pad  or hardware pedistal and a bronze halyard winch if the two are bolted directly together.  A thin layer of plastic between the two  virtually eliminates this problem, particularly if you use an anti-sieze on bolt (typically stainless) threads.  I use lanolin anti-sieze commonly found in boating stores.  My favorite barrier material is easy and cheap to make.  Prepare a smooth surface with mold release wax, lay a section of a light fiberglass cloth (say an 8 oz) and saturate with a laminating epoxy such as West Systems or System Three.  You now have a sheet of flexible barrier material which can be cut to size as needed.

 

  • Thanks 1
  • Like 2
Posted
6 hours ago, Jim and Frances said:

I removed our bike rack factory installed 1.5" receiver and noticed some corrosion on the underside of the rack where the u-bolts/washer attach .  Will be checking other fasteners / washers going through the aluminum members around the bumper/bike rack area and adding some thin delrin/acetal washers to put under the stainless washers and maybe adding a thin coat of Ultra Tef-Gel to the hole walls  -OR- should I do something different? 

image.png.efe49abb81ba75e2fcd10e44d69ce4e0.png

This is on my to-do list.

  • Like 1

2014 Ram 2500 Cummins Diesel 4X4 Truck

2024 Oliver Legacy Elite II Hull 1460

ARILINIAKSKYLAMIMNMOOHOKTNTX00CC66med.jp

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
×
×
  • Create New...